Black Friday Is Here! Shop Unbelivable Offers & Take 20% Off Almost Everything Else!
Use Code: BLKFRI20

Black Friday Is Here! Shop Unbelivable Offers & Take 20% Off Almost Everything Else!
Use Code: BLKFRI20

ALUMA-HYDE® II

ALUMA-HYDE® II Reviews & Ratings

Brownells Aluma-Hyde II is a durable, epoxy-based aerosol firearm finish developed to resist bore cleaners, solvents, cleaning chemicals, and everyday wear. Formulated with a hard-curing epoxy base and high-density pigments, it provides a protective, abrasion-resistant coating for properly prepared aluminum, steel, alloys, and synthetic surfaces.

Unlike conventional finishes that can be damaged by aggressive cleaning chemicals, Aluma-Hyde II offers increased chemical resistance after fully curing. It is resistant to many common bore cleaners and solvents, although particularly aggressive copper-removing solvents may affect the finish.

Available in a variety of colors, Aluma-Hyde II can be used to refinish firearm components, synthetic stocks, and other compatible surfaces. No primer is required on properly prepared bare metal or anodized surfaces.

Aluma-Hyde II Features & Specifications

  • Hard-curing epoxy-based aerosol finish
  • Resistant to common bore cleaners and solvents after curing
  • Durable, abrasion-resistant protective coating
  • Adheres to properly prepared aluminum, steel, alloys, and plastics
  • Suitable for compatible synthetic stocks and fiberglass surfaces
  • No primer required on properly prepared bare metal or anodized surfaces
  • Available in multiple colors
  • 12 oz. (340 g) aerosol can
  • Includes a Clean Out Nozzle for clearing the pickup tube

Aluma-Hyde II Colors & Finish Examples

Compare Aluma-Hyde II colors applied to actual magazines. The examples below show how different finishes appear on the same type of surface.

Brownells Aluma-Hyde II color comparison showing different finishes applied to firearm magazines
Aluma-Hyde II colors shown on coated magazines. Actual appearance may vary with lighting, screen settings, surface preparation, and application.

View more Aluma-Hyde II colors and finished project photos in our product spotlight.

How to Apply Aluma-Hyde II

Surface preparation, application temperature, and curing all affect the finished coating. Follow the instructions below and consult the product label and safety information before use.

Step 1: Prepare the Surface

Surfaces must be completely dry and free of oil, wax, dirt, loose paint, and other contaminants. No primer is required on properly prepared bare metal or anodized surfaces.

Clean previously painted surfaces with a suitable cleaner or degreaser. If abrasive blasting, ensure the blasting media is free of oil and silicone. Always test a small area for color compatibility and adhesion.

Preparation varies by material:

  • Unpainted Aluminum: Abrasive blast to achieve the desired surface texture.
  • Unpainted Steel: Remove rust by sanding or abrasive blasting.
  • Fiberglass: Sand lightly, then wash with soap and water or a quality cleaner/degreaser.
  • Wood: Seal or fill the surface before application. Aluma-Hyde II can be applied over polyurethane and varnish finishes, but not over linseed oil or tung oil finishes.

Watch our Aluma-Hyde II surface preparation video for a demonstration of proper preparation techniques.

Step 2: Prepare the Aerosol Can

For best results, apply Aluma-Hyde II at temperatures between 70°F and 90°F. Do not apply below 65°F.

Shake the can vigorously until the mixing ball rattles, then continue shaking for an additional two minutes to ensure consistent color and texture.

Use the included Clean Out Nozzle before each use. Remove the standard spray nozzle and install the Clean Out Nozzle. Point the can in a safe direction and depress the valve to clear accumulated paint or residue from the pickup tube.

Once the discharge is clear and consistent, remove the Clean Out Nozzle and replace the standard spray nozzle before applying the finish. The Clean Out Nozzle is not intended for finish spraying.

Step 3: Apply Aluma-Hyde II

Hold the aerosol can approximately 12 inches from the prepared surface and fully depress the spray valve. Shake the can periodically during application to maintain consistent color and texture.

If additional coats are required, apply them within the initial 30-minute recoating window. After that window has passed, allow the coating to cure for 10 to 14 days before applying another coat.

Watch our Aluma-Hyde II application video for additional spraying techniques and application tips.

Step 4: Allow the Finish to Cure

Allow the coating to cure fully before putting the finished part into service. Drying and curing times vary depending on coating thickness, temperature, and humidity.

  • Touch Dry: Approximately 10 to 15 minutes.
  • Handling: Wait at least 24 hours before extensive handling.
  • Recoating: Apply additional coats within 30 minutes, or allow 10 to 14 days of curing before recoating.
  • Air Curing: Circulating warm air up to 90°F or placing the part in direct sunlight can help reduce curing time.
  • Accelerated Curing: Existing product instructions specify baking the coated part for 3.5 hours at 195°F. This method is appropriate only for heat-tolerant components and must follow applicable product safety instructions. Allow the part to cool before recoating.

Clean Out Nozzles & Maintenance

Each can of Aluma-Hyde II includes a Clean Out Nozzle designed to clear partially hardened paint from the pickup tube and help prevent clogs, sputtering, and inconsistent spray patterns.

Additional Clean Out Nozzles are available separately:

  • Single Clean Out Nozzle: Item #430107431
  • 12-Pack Clean Out Nozzles: Item #084179004

Clean Out Nozzles are for clearing the pickup tube only and are not intended for finish spraying.

Aluma-Hyde II Application Guides & Videos

Brownells Gun Tech Caleb Savant demonstrates surface preparation, application, camouflage patterns, and other finishing techniques in our instructional series.

Watch the complete How to Paint Your Firearm video series

View Product
Write a review
Reviews Summary
Aluma-Hyde® II garners mixed feedback, with many users appreciating its cost-effectiveness and ease of application, while others encounter issues with nozzle clogging and inconsistent color matching, particularly with the FDE variants. Durability after curing is generally praised, though some users report chipping and flaking over time. Overall, users recommend proper prep and caution for the best results.
What Reviewers Are Saying
Application Process
70%
Many reviewers emphasize the importance of following the application instructions precisely, including thorough cleaning and allowing adequate cure time. Users highlight that successful application often requires shaking the can extensively and avoiding excessive heat when curing.
Durability
65%
The durability of Aluma-Hyde® II is frequently mentioned, with many users noting it holds up well under regular use. However, some express disappointment when experiencing chipping or wear, especially in high-friction areas.
Color Match
60%
Color consistency is a significant concern. Several users report discrepancies between the color on the cap and the actual paint, particularly with variants like Coyote and FDE. Aluma-Hyde II is described as closer to Sage or light tan rather than the expected hues.
Nozzle and Clogging Issues
55%
Numerous reviews highlight issues with the spray nozzles clogging shortly after use, leading to spattering or inconsistent application. Users recommend purchasing extra nozzles as a precaution.
Value for Money
75%
Despite the mixed feedback, many users find Aluma-Hyde® II to be a cost-effective alternative to professional coatings like Cerakote. The majority feel that it delivers adequate performance for the price, especially for DIY projects.
1
GARBAGE
I can't understand how anyone gives this garbage a positive review. I ordered a can, immediately had clogging issues despite shaking it up. Ruined the finish on a gun and I had to sandblast and redo it (I parkerized it instead). Decided I maybe hadn't shaken it up enough, so I bought another can to try on a different rifle. Shook it up for around 10 minutes solid. Just sat there watching TV shaking it. Tried it out on some cardboard until I thought it was going good. Started on the rifle, halfway through - clogs and begins spraying out chunks that stuck to the rifle barrel. I was shaking it the entire time I used it as well. I essentially have now RUINED the finishes on two separate projects that I have to re-sandblast and re-do, costing hours of labor not even mentioning the 30 bucks for the cans. Do yourself a favor, use Gunkote instead. It actually works.
1
Unreliable nozzle
I bought 4 cans of matte black and 3 out of the 4 had serious issues with the nozzle. They either wouldn't spray or would spit paint in globs, giving an uneven, runny finish. The paint itself is great, but the nozzle/flow system is terrible.
1
Never again.
I used my first can of Aluma-Hyde II weeks ago to refinish an old rifle. I followed the instructions for use.. shook the can for probably 5 minutes before trying to apply. The nozzle on the can clogged often, making for drips and uneven spray patterns, and then eventually broke completely. I ordered a second can last week to try to finish the restoration project but was disappointed when this can also spurted out uneven chunks and eventually started spewing out of the top of the can. The material itself seems durable enough though after drying in front of a fan for about a week.
1
Not Bad. When the Nozzle Works.
The product clogs in the nozzle, even though it was shaken for a full 10 minutes prior to application. I got half way through refinishing a rifle and then it just stopped spraying. I cleaned the nozzle with Gumout spray carb cleaner and the nozzle began working for another 20 seconds. It screwed up my entire project and now I have to strip this fecal matter off and find another coating. I think I'll try Krylon spray paint. At least that sprays when I push the nozzle.
1
Don't waste your money
Used as directed, didn't even get one coat before the nozzle clogged up. Had to keep cleaning the nozzle with a needle then after 2 coats the can clogged completely.
1
doesn't stay on the metal
followed instructions and let sit in my spare bathroom with a heater running. after four days i can scrape the paint off with a fingernail. great big waste of time and money.
1
will not work most of the time
I have ordered several cans over the years and have had good and bad results the bad being the more of the 2 with this. Its good paint but the cans clog after a minute or so of use. Then you have to purchase extra nozzles and that doesn't work either. then you have to order clean out nozzles to get the paint out of the can. Bottom line is don't buy it your wasting your time with it.
1
A whole week...who has time for this?
Takes an entire week to dry. If you touch the part before the week, it is very soft and leaves a smudge. If you try to move the part it will smudge. Try to touch-up the bad spot? oh gotta wait another week for that also. Need to flip the part over to spray the bottom/back side? Gotta wait another week for that. Who has time for all that? Need extra shop space just waiting on all parts to dry. Seriously Brownells: need to make a formula that is ready-to-go after 24 hours. Credit where credit is due: Brownell's did refund my money, no problems, thanks.
1
came with broken nozzle, wouldnt spray
TOTAL GARBAGE. came from Brownells with a bad nozzle and no matter how good the product inside is,and it is good product,its TOTALLY WORTHLESS if you cant get it out of the can. Lucky i tested it on smaller project or it would have dribbled out and caused havoc on my real reason for buying it. what a let down.
1
Never again
I will never order this product again. I will use Krylon/Rustoleum/anything else instead. The first thing I noticed was that it clogs up the nozzle quickly. As in during the coat while spraying. Shake the can as much as you want, you will start getting an uneven spray or no spray at all in the middle of your coat. You will have to take the nozzle off to clean it during spraying. The second can I used had a faulty nozzle from the beginning. When this happened during my second coat, I tried to gently wipe it clean, only to have the prior coat come up, after drying for 48+hours in a heated room. If you decide that you just can't live without this product, order spare nozzles by the truckload, and be prepared for frustration.